German Technical Background VOK-204 Wetting Dispersant Control Flocculation and Prevent Floating Color Replaces BYK-204
German technical background VOK ®- Disper 204 Wetting Dispersant
VOK ®- Disper 204 Controlled flocculation wetting dispersant for solvent based systems, used to prevent the settlement of fillers and inorganic pigments in medium polar to non-polar thick coating systems and primers, and the preparation of bentonite slurry
Product Information
Chemical composition
Polycarboxylate solution of polyamine amide
Typical Physicochemical Data
The data given in this data page are only typical values, not technical indicators of the product.
Amine value: 37 mg KOH/g
Acid value: 41 mg KOH/g
Density (20 ° C): 0.93 g/ml
Non volatile matter (20 minutes, 150 ° C): 52%
Solvent: propylene glycol methyl ether/alkylbenzene 3/2
Flash point: 31 ° C
Application information
Coating industry
Features and Benefits
The additive plays a role by controlling flocculation of pigments. The flocculation control function can also resist sagging, prevent pigment sedimentation and floating color.
And VOK ®- Disper 203 is different, VOK ®- Disper 204 is also suitable for nonpolar systems (compatible with petroleum solvents). The lower the polarity, the stronger the thixotropy. Suitable for long oil, medium oil and short oil alkyd, PVC copolymer, chlorinated rubber and epoxy base material systems. When used as anti-corrosion primer, the anti-corrosion performance is often improved.
Recommended Applications
Particularly recommended application fields: industrial coatings, wood and furniture coatings, anti-corrosion coatings.
Recommended application field: architectural coatings.
Recommended dosage
Additive dosage (purchase form) is based on pigment:
Inorganic pigment: 1-2%
Titanium dioxide/filler: 0.5-1%
Bentonite: 30-50%
The above data are empirical dosage, and good dosage shall be determined through a series of tests.
Addition method and processing guidance
In order to obtain good performance, the additive should be added to the abrasive first, and then the pigment.
The additive can remedy the paint with problems, but its efficacy will be reduced at this time.
Recommended formula of bentonite slurry:
85-87 parts by weight of solvent
10 parts by weight of bentonite
5-3 parts by weight of additives
The solvent can be aromatic solvent or aromatic petroleum solvent, or aromatic free solvent gasoline. If the gel effect is insufficient, polar solvent can be added to enhance the gel effect.
Special attention
In coatings based on nitrocellulose, chlorinated rubber or polyvinyl chloride copolymer, these additives may cause discoloration. In the silicate coating, the construction time limit will be shortened. Higher addition may affect the construction time limit and curing reaction of epoxy system. The amine value of the additive is high, which will cause the viscosity of epoxy resin to increase.
SMC, BMC, pultrusion
Features and Benefits
The additive plays a role by controlling the flocculation of the filler and is mainly used to prevent the settlement of the filler.
Recommended Applications
Particularly recommended application field: pultrusion.
The additive is applicable to all pultrusion resin systems including unsaturated polyester, vinyl ester, acrylic acid and epoxy.
Recommended dosage
0.5-1.5% auxiliary dosage (purchase form) based on filler
The above data are empirical dosage, and good dosage shall be determined through a series of tests.
Addition method and processing guidance
In order to obtain good performance, the additive should be added to the grinding material first, and then added with pigments and fillers.
Room temperature curing system
Features and Benefits
The additive plays a role by controlling the flocculation of fillers and tablets, and is mainly used to prevent particle sedimentation. ANTI-TERRA-204 can make the filler and sheet in acrylic acid system more uniform. The additive can prevent sedimentation, and the system using flakes can obtain a more even surface structure.
Recommended Applications
Particularly recommended for acrylic systems (PMMA in MMA).
Recommended dosage
0.5-1.5% auxiliary dosage (purchase form) based on filler
The above data are empirical dosage, and good dosage shall be determined through a series of tests.
Addition method and processing guidance
In order to obtain good performance, the additive should be added to the abrasive first, and then the powder.
Send Inquiry to This Supplier
You May Also Like
-
German Technical Background VOK-U80 Wetting Dispersant Inorganic Pigment in Stable Solvent System Replaces BYK-U80CNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-U100 Wetting Dispersant Increase Color Intensity Replaces BYK-U100CNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-UMEN Wetting Dispersant Increase Luster While Preventing Sedimentation and Sagging Replaces BYK-UMENCNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-250 Wetting Dispersant Scratch Resistant and Easy to Clean Replaces BYK-250CNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-I Wetting Dispersant Improve Tinting Intensity Replaces BYK-ICNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-U100 Wetting Dispersant Increase Color Intensity Replaces BYK-U100CNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-1000 Wetting Dispersant Improve Surface Protection Performance and Touch Replaces BYK-1000CNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-220S Wetting Dispersant Improved Gloss and Leveling of Paint Replaces BYK-220SCNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-198 Wetting Dispersant Good Flow Performance Replaces BYK-198CNY 150 - 180MOQ: 25 Kilograms
-
German Technical Background VOK-2012 Wetting Dispersant Improve Color Intensity and Transparency Replaces BYK-2012CNY 150 - 180MOQ: 25 Kilograms