No. | Item | Test Value | |||||||||
0.75mm | 1.0 mm | 1.25 mm | 1.5 mm | 2.0 mm | 2.5 mm | 3.0mm |
|
|
| ||
1 | Minimum Density(g/cm³) | 0.939 | |||||||||
2 | Tensile Property | ||||||||||
Yield Strength ,N/mm | 11 | 15 | 18 | 22 | 29 | 37 | 44 |
|
|
| |
Break Strength ,N/mm | 20 | 27 | 33 | 40 | 53 | 67 | 80 |
|
|
| |
Yield Elongation ,% | 12 | ||||||||||
Break Elongation ,% | 700 | ||||||||||
3 | Tear Resistance N | 93 | 125 | 156 | 187 | 249 | 311 | 374 |
|
|
|
4 | Puncture Resistance N | 240 | 320 | 400 | 480 | 640 | 800 | 960 |
|
|
|
5 | Stress Crack Resistance, hrs | 300 | |||||||||
6
| Carbon Black | ||||||||||
Carbon Black Content, % | 2.0-3.0 | ||||||||||
Carbon Black Dispersion | Carbon black dispersion(only near spherical agglomerates) for 10 different views 9 in categories 1 or 2 and 1 in category 3 | ||||||||||
7
| Oxidative induction time(OIT) | ||||||||||
Standard OTI Min | 100 | ||||||||||
High Pressure OTI Min | 400 | ||||||||||
8 | Oven aging at 85℃ | ||||||||||
Standard OIT-% retained after 90 days | 55 | ||||||||||
High pressure OIT-% retained after 90 days | 80 | ||||||||||
9 | UV Resistance | ||||||||||
Standard OIT retained after 1600 hrs | 50 | ||||||||||
High pressure OIT retained after 1600 hrs | 50 | ||||||||||
10 | Low tempreture impact brittle property at -70°C | Pass | |||||||||
11 | Water vapor permeability (g.cm/cm2 .s.Pa) | ≤1.0×10-13 | |||||||||
12 | Dimensional Stability (%) | ±2 | |||||||||
HDPE Geomembrane Roll Size HD
Thickness | Width | Length | Remark |
0.5mm | 5.8m ( Standard ) | 50m - 400m | The standard width is based on the max loading quantity according to the container size . It’s will be loading more quantity to save Freight cost .
For other types also could be produce as request , the exact package will send to you driectly . |
7.0m | 50m - 400m | ||
7.5m | 50m - 400m | ||
8.0m | 50m - 400m | ||
1.0mm | 5.8m ( Standard ) | 50m / 100m / 150m | |
7.0m | 50m / 100m / 150m | ||
7.5m | 50m / 100m / 150m | ||
8.0m | 50m / 100m / 150m | ||
1.5mm | 5.8m ( Standard ) | 50m / 100m / 140m | |
7.0m | 50m / 100m/ 140m | ||
7.5m | 50m / 100m/ 140m | ||
8.0m | 50m / 100m/ 140m | ||
2.0mm | 5.8m ( Standard ) | 50m / 100m | |
7.0m | 50m / 100m | ||
7.5n | 50m / 100m | ||
8.0m | 50m / 100m |
Function HDPE g
- 1. Good flexibility
2. For service temperature range : -70℃ ~ +110℃
3. Corrosion resistance , aging resistance
4. Excellent environmental stress cracking resistance property
5. High tensile strength and elongation
Application HDPE geomembrane price
1.Landfills , sewage or waste treatment sewage.
2.River bank, lake dam, dam, water dam and reservoir, channel,has liquid pool ( pit , mine )
3.Metro , basements and tunnels , tunnel seepage control liningfoundation and other foundation saline seepage.
4.Embankment, upstream impervious blanket level, foundation
vertical impermeable layer, cofferdam construction, waste disposal.
5.Sea water, fresh water fish farm.
6.Road , highway , railway foundation expansive soil and loess of the waterproof layer.
7.Roof impervious.
Send Inquiry to This Supplier
You May Also Like
-
CE and ASTM Self Bituminous Adhesive Waterproof Membrane for Roof, Window, Door, Road, Bridge, Ship Deck Anti Corrosion Protection Pipe TapeNegotiableMOQ: 100 Rolls
-
Non-curable Rubber Modified Asphalt Coating for WaterproofingUS$ 1.5 - 6MOQ: 500 Kilograms
-
Low Cost Waterproof Material ManufactureUS$ 1,000 - 50,000MOQ: 1 Set
-
Cheap Price Diesel Engine M11 3080760 Cylinder LinerUS$ 27 - 29MOQ: 6 Pieces
-
2000 Cups Membrane Film Different Color Sealing Cup Sealing MachineUS$ 88.2 - 112MOQ: 12 Rolls
-
Adjustable Aluminum Alloy Rope Suspended Platform ZLP 800 For Refurbishing / PaintingNegotiableMOQ: 1 Meter
-
PTFE Architectural Membrane MaterialNegotiableMOQ: 1
-
Sell SBS Waterproof Sheet MaterialsNegotiableMOQ: 1 Meter
-
Special Compound BaseUS$ 0.12 - 0.25MOQ: 7000 Square Meters
-
Concrete Embedment Strip for Waterproof Geomembrane LinersNegotiableMOQ: 1 Piece