Shrimp Pond Waterproofing Plastic Sheet in Rolls

Shrimp Pond Waterproofing Plastic Sheet in Rolls photo-1
US$ 0.15 - 3.8 MOQ: 1000 Square Meters
Key Specifications
Get Latest Price
Place of Origin:
Shandong, China
Brand Name:
Jinruixiang
Model Number:
0.5mm
Payment & Shipping
Payment Methods:
Port of Shipment:
Qingdao
Delivery Detail:
Delivery time depends on order quantity.
Place of Origin Shandong, China
Brand Name Jinruixiang
Model Number 0.5mm
Material HDPE

 

 

 
Product Description

 

ProductHigh Quality HDPE Pond Liner
Material97.5% of high-density polyethylene resin and 2.5%of carbon black/antiaging agent/anti-oxygen/UV absorber/stabilizer and other adjuvant
Thickness0.2mm-2.0mm
ColorBlack/green/blue
SurfaceBoth side smooth/both side textured/one side textured
QualityGB standard/GM13
ApplicationArtificial lake,pond,domestic garbage landfill,mining&chemical industry,roof garden,fish pond,reservoir etc.

High Density Polyethylene Geomembrane with Environmental Smooth Surface (GB/T 17643-2011 GH-2)

 

S/N

 

Item

Index

Thickness mm

0.75

1.00

1.25

1.50

2.00

2.50

3.00

1

Density

g/cm3

≥0.940

2

Tensile yield strength (vertical and horizontal)

N/mm

≥11

≥15

≥18

≥22

≥29

≥37

≥44

 

3

Tensile breaking strength (vertical and horizontal)

N/mm

≥20

≥27

≥33

≥40

≥53

≥67

≥80

4

Elongation (vertical and horizontal)

%

-

-

-

≥12

5

Elongation at break (vertical and horizontal)

%

≥700

6

Tearing load at right angle (vertical and horizontal) N

≥93

≥125

≥160

≥190

≥250

≥315

≥375

7

Anti-puncture strength

N

≥240

≥320

≥400

≥480

≥540

≥800

≥960

8 '

Tensile load stress cracking (tensile method of dead load of the cut)

h

_

≥300

9

Carbon black content

%

2.0~3.0

10

Carbon black dispersion

The number of Level 3 among 10 data is not more than one; Level 4 and Level 5 are not allowed.

 

Oxidation induction time (OIT)

min

Oxidation induction time under normal pressure ≥100

11*

Oxidation induction time under disjoining pressure ≥400

12

85°C thermal aging (retention rate of OIT under normal pressure after 90d) %

≥55

13a

Ultraviolet resistance (retention rate of OIT after 1600h ultraviolet irradiation)

%

≥50

 Note: Technical performance index of thickness specification not listed in the table shall be implemented according to interpolation method.

For two indexes of Item 11 and Item 13, select one from retention rate of OIT under normal pressure and retention rate of OIT under high pressure and carry out the test.

 

Company Information

shrimp pond waterproofing plastic sheet in rolls

FAQ

  1.Q:How about your raw material?

   A:The raw material is 97.5% high quality high-density polyethylene resin and 2.5% of carbon black,and 100% original raw material.

 

2.Q:How about your production capability?

   A:The daily capability is 14T/day.And we have already installed another one production line which the daily capability can reach 25T/day.

 

3.Q:Is it difficult to install?Will you provide installation serivce?

   A:The installation method for HDPE geomembrane is hot welding which need specical machine.We have several experienced elding engineers who have rich installation experience.Professional suggestion and installtion will be provided to you if you need.

Send Inquiry to This Supplier

Message
0/5000
Want the best price? Post an RFQ now!
Business Type
Manufacturer, Trading Company
Year Established
2009
Factory Size
10,000-30,000 square meters
Total Employees
201 - 300 People

Recommended Categories

Explore top categories and find suppliers for your specific needs