SK 34 Refractory Fire Clay Brick

SK 34 Refractory Fire Clay Brick photo-1
SK 34 Refractory Fire Clay Brick photo-2
SK 34 Refractory Fire Clay Brick photo-3
SK 34 Refractory Fire Clay Brick photo-4
SK 34 Refractory Fire Clay Brick photo-5
SK 34 Refractory Fire Clay Brick photo-6
US$ 150 - 260 MOQ: 1 Ton
Key Specifications
Get Latest Price
Place of Origin:
Henan, China
Shape:
Brick
Material:
Alumina Block
Payment & Shipping
Payment Methods:
Port of Shipment:
Tianjin Qingdao Shanghai
Delivery Detail:
Delivery time depends on order quantity.
Place of Origin Henan, China
Shape Brick
Material Alumina Block
SiO2 Content (%) 40%~43%
Al2O3 Content (%) 55%~58%
MgO Content (%) 0.8-1.2
CaO Content (%) 0.01
CrO Content (%) 0.1~0.3%
SiC Content (%) 0.00%
Model Number SK34
Brand Name Dengda
SK34 Description

 SK 34 refractory fire clay brick

SK34 Firebrick 
1 Al2O3: 50~55% 
2 Standard size in stock 
3 Special shape available 
4 Factory supply&Reliable quality

Factory supply refractory firebrick  SK34

 

Category of Refractory Brick/Fire Brick:

 

a) According the made method, it can be divided into burnt brick, unburned brick, and electric smelting brick.

b) According the shape and size, it can be divided into standard brick, general brick and abnormal shape brick.

c) According the content of the Al2O3, it can be divided into fire clay brick and high alumina firebrick.

 

Firebrick SK34 Index

  SK 34 refractory fire clay brick

Item

SK38

   SK37

SK34

SK34

Al2O3  %

≥75

≥65

≥55

≥48

Cold crushing strength ,MPa

≥54

≥49

≥44

≥40

Apparent porosity  ,%

≤23

≤23

≤22

≤22

Refractoriness under load , °C

≥1520

≥1500

≥1470

≥1420

Reheating linear change (1500°C,2h) %

+0.1-0.4

+0.1-0.4

+0.1-0.4

(1450°C,2h)+0.1-0.4

Refractoriness  °C

>1790

>1790

>1770

>1750

SK 34 refractory fire clay brick

Applications of Refractory Firebrick SK34 

1.  Carbon bake furnace in the aluminium industry

2.  Preheat zones and cyclones of rotary cement kilns

3.  Primary reformers in fertilizer production

4.  Insulation for glass tanks

5.  Coke ovens

6.  Blast furnace

7.  Reheating furnace

8.  Suspended roofs

9.  Lime kilns

10. Domestic fireplaces, barbeques and outdoor ovens

 Production process of Refractory Firebrick SK34

1) Generally, Rrfractory firebrick SK36  was molded by dry pressing.

2) By means of mixing the material uniformity in proportion and ageing mixture some time. Then, pour some powders into the mold and dry pressing.

3) After dry pressing, the adobe needs to be pushed in the drying kiln to stove or stay in the air to dry. This progress will need about 3-5 days.

4) After this progress, then push the adobe into the tunnel furnace or shuttle kiln to burn around 1300C. This progress will be need about 5-7 days.

5) After burning, the finished Rrfractory Firebrick SK36  will be packed on pallet.

Size of Refractory Firebrick SK34
Shape is  available according to your drawings.

Packaging & Shipping

  The Rrfractory firebrick SK34 are packed on stadard export wooden pallet with papers in each layer, thick paper on the five sides, and PVC film wrapped outside of the whole pallet.

SK 34 refractory fire clay brick

 

Company Information

 SK 34 refractory fire clay brick

SK 34 refractory fire clay brick

SK 34 refractory fire clay brick

 

Our Services

1. Dengda enterprise is refractory business mogul in China.

2. Quality is our culture.
3. Our sales pitch is with us your money in safe your business in safe.
4. We have professional automatic production line and stuff who is making high quality in short time.
5. We will sign contract with you to be more safe.
6. We produce according to your detail specifications.
7. The good business start here!

Send Inquiry to This Supplier

Message
0/5000

Want the best price? Post an RFQ now!
Business Type
Manufacturer, Trading Company
Year Established
2001
Factory Size
Above 100,000 square meters
Total Employees
501 - 1000 People

Recommended Categories

Explore top categories and find suppliers for your specific needs